High pressure easy dart
Posted: Fri Sep 04, 2009 11:26 pm
I decided not to search the entire forum to see if this has already been posted, so if it has consider this an update.
My launcher has a blow gun barrel so I could use blow gun darts, but I use 400 psi. The cones deform at that pressure and fly erratic.
This is my fix.
The tubing used is nylon. The larger tube is 6.5 Mm Id, 10 Mm Od, and fits perfect in a 40 cal. blowgun. It fits a little lose over the small tube but if it fit any tighter it would be hard to slip it on with super glue on it. The small tube is 1/4" Od, 1/8" Id, and fit tight over the shaft. I had to get some vice-grips and force the shaft into the tube.
So, I cut a bunch of small tubes at 3/8 inch and the big tubes at 1/2 inch. Slip the small tube so the shaft is 3/4 the way thru it. then put the big tube about 3/4 the way over the small tube, as shown in the pic. use super glue on the shaft and between the tubes. let it dry for 24 hrs. If you don't you will get bugers when you try to grin it. Also make sure you run the drill in reverse or the opposite way the grinding wheel is turning. This will help keep plastic burrs cleaned off.
These cones will not collapse. At 400 psi the dart will go clean through a solid 2x10 from 50 feet away. The cones of coarse pop off.
The larger darts in the picture (pistol crossbow bolts) will pearce just through the other side.
My launcher has a blow gun barrel so I could use blow gun darts, but I use 400 psi. The cones deform at that pressure and fly erratic.
This is my fix.
The tubing used is nylon. The larger tube is 6.5 Mm Id, 10 Mm Od, and fits perfect in a 40 cal. blowgun. It fits a little lose over the small tube but if it fit any tighter it would be hard to slip it on with super glue on it. The small tube is 1/4" Od, 1/8" Id, and fit tight over the shaft. I had to get some vice-grips and force the shaft into the tube.
So, I cut a bunch of small tubes at 3/8 inch and the big tubes at 1/2 inch. Slip the small tube so the shaft is 3/4 the way thru it. then put the big tube about 3/4 the way over the small tube, as shown in the pic. use super glue on the shaft and between the tubes. let it dry for 24 hrs. If you don't you will get bugers when you try to grin it. Also make sure you run the drill in reverse or the opposite way the grinding wheel is turning. This will help keep plastic burrs cleaned off.
These cones will not collapse. At 400 psi the dart will go clean through a solid 2x10 from 50 feet away. The cones of coarse pop off.
The larger darts in the picture (pistol crossbow bolts) will pearce just through the other side.